Production process: high purity magnesia and high purity synthetic dolomite sand as the main raw materials, at the same time adding wetting agent and sintering agent by hot mixing.
Main application: hot repair of converter surface.
Usage method: When repairing a large area, pour -200-300kg (according to the size of the converter and the degree of erosion and area of the lining brick) of the large surface hot repair material into the furnace with a chute to repair the part, sintering 10-30 minutes (according to the thickness of the repair material) can be used; For small area local repair, our company produces 10kg/ bag and 5kg/ bag of hand-cast hot repair materials according to the use habits of steel mills, which can be selected according to the specific situation of the repair parts.
Product code | MgO% | SiO2% | Fe2O3% | CaO% | C% | B.D.g/cm³ |
---|---|---|---|---|---|---|
ZDML-1 | ≥76 | ≤2.5 | ≤2.0 | ≤3.0 | 4-6 | ≥2.4 |
ZDML-2 | ≥80 | ≤2.0 | ≤1.8 | ≤3.0 | 4-6 | ≥2.5 |
ZDML-3 | ≥82 | ≤1.5 | ≤1.5 | ≤3.0 | 4-6 | ≥2.6 |
ZDBL-1 | 72-76 | ≤1.0 | ≤1.0 | 9-11 | 4-6 | ≥2.5 |
ZDBL-2 | 76-80 | ≤1.2 | ≤1.2 | 6-8 | 4-6 | ≥2.5 |