Production process:It is made of high quality magnesia and calcined olivine as the main raw materials, and mixed with a variety of binders.
Main application:Thousand pound for tundish working layer.
Usage method:The dry material is rammed in the mold, and then heated and cured, and the curing temperature is between 230-300℃. Depending on the raw material, the service life is generally between 70-90 hours.
Product code | MgO% | SiO2% | Fe2O3% | CaO% | Changes in line after burning (1500℃x2h)% |
---|---|---|---|---|---|
ZBGL-1 | ≥82 | ≤4 | ≤1.5 | ≤2 | ≤-4% |
ZBGL-2 | ≥65 | 18-22 | 3-5 | ≤2 | ≤-5% |